How to use this tool
- Measure the worn slab — length × width of the area to be overlaid.
- Set thickness. Polymer-modified resurfacers go on ⅛–½ in; the tool defaults to ½ in. Thin skim coats need far less material.
- Check the product data sheet for square feet per bag at that thickness and enter it — brands differ widely.
- Enter bag price for the material total. Labor is the bigger line on resurfacing, and it is usually quoted per square foot.
How the result is calculated
Volume (ft³) = length (ft) × width (ft) × thickness (ft) × number of areas, multiplied by your waste factor, then divided by 27 for cubic yards. Circular areas use π × (diameter ÷ 2)². Bag counts use standard US yields: an 80 lb bag yields about 0.60 ft³ of mixed concrete, a 60 lb bag about 0.45 ft³.
Choosing the right numbers
Resurfacing is a surface repair, not a structural one. It succeeds when the slab underneath is sound, and fails wherever it is not:
- Good candidates: sun-faded color, minor surface spalling, old stains, worn broom texture.
- Bad candidates: heaving or settled slabs, working cracks, or slabs that dust (chalky surface). Fix the cause first or the overlay follows it down.
- Prep is the job: pressure wash, degrease, and profile the surface. Resurfacer bonds to a clean roughened slab, not to a shiny sealer or loose dust.
- Control joints must be preserved. Mask and work around them, or the overlay bridges the joint and cracks there anyway.
Typical coverage at ½ in: a 50 lb bag of polymer resurfacer covers roughly 25–40 sq ft depending on mix water. A two-car driveway (≈ 400 sq ft) runs 10–16 bags per coat.
Common mistakes to avoid
- Overlaying unsealed cracks. Any moving crack reflects through the overlay within months. Repair with crack filler first, and expect movement cracks to reappear.
- Skipping the primer/bond coat. Most systems need a bonding primer or a scratch coat on porous slabs.
- Too much mix water. Soupy mix is easier to spread and weaker when cured — it dusts and flakes. Follow the sheet, not your arm.
- Working alone in the sun. Resurfacer sets fast; one person can barely cover 100 sq ft before the bucket stiffens. Two people, one mixing and one placing.
Worked examples
Example — 12 ft × 14 ft patio overlay, ½ in, 30 sq ft per bag
Area = 168 ft²; with 10% waste ≈ 185 ft². Bags = 185 ÷ 30 = 6.2 → 7 bags. At $30 a bag, about $210 in material. (The tool's concrete-volume output still shows the overlay in yards for comparison — about 0.31 yd³.)
Frequently asked questions
How much resurfacer do I need per square foot?
It depends on the product and thickness — a typical 50 lb polymer bag covers 25–40 sq ft at ½ in, or considerably more as a thin skim coat. Check the data sheet and enter its coverage figure.
Can I resurface a cracked driveway?
Only after repairing the cracks. Static cracks filled with rigid repair material can be overlaid; moving or structural cracks will telegraph through any thin overlay.
Is resurfacing cheaper than repouring?
Usually yes for cosmetic problems — material runs a fraction of a new pour, though labor still dominates. If the slab is settling, heaving or structurally cracked, replacement is the durable answer.
Assumptions, sources and limits
- Coverage per bag comes only from your product data sheet — the tool does not assume a brand.
- One coat only; texture coats and decorative finishes are separate passes with their own coverage.
- Adhesion assumes sound, cleaned, profiled concrete. Resurfacing does not fix structural problems.
Planning estimates only; follow the manufacturer's installation sheet.